Title | Mitigation of the irreversible capacity and electrolyte decomposition in a LiNi0.5Mn1.5O4/nano-TiO2 Li-ion battery |
---|---|
Publication Type | Articolo su Rivista peer-reviewed |
Year of Publication | 2011 |
Authors | Brutti, S., Gentili V., Reale P., Carbone L., and Panero S. |
Journal | Journal of Power Sources |
Volume | 196 |
Pagination | 9792-9799 |
ISSN | 03787753 |
Keywords | Anode side, Cathode materials, Cathodes, Charge loss, Coin cells, Electrolyte additives, Electrolyte decomposition, Electrolytes, Energy density, Ex situ, First cycle, Innovative approaches, Ion exchange, Ions, Irreversible capacity, Irreversible capacity loss, Li-ion batteries, Li-Ion cells, LiNi<sub>0.5</sub>Mn<sub>1.5</sub>O <sub>4</sub>, Liquid electrolytes, Lithium, Lithium-ion battery, Manganese, Manganese oxide, Manganese spinels, Nano-sized, Rate capabilities, Reversible specific capacity, Surface reactivity, TiO, Titanium, Titanium dioxide, Zinc oxide, ZnO |
Abstract | Nanosized titanium oxides can achieve large reversible specific capacity (above 200 mAh g-1) and good rate capabilities, but suffer irreversible capacity losses in the first cycle. Moreover, due to the intrinsic safe operating potential (1.5 V), the use of titanium oxide requires to couple it with high-potential cathodes, such as lithium nickel manganese spinel (LNMO) in order to increase the energy density of the final cell. However the use of the 4.7 V vs. Li+/Li0 LNMO cathode material requires to tackle the continuous electrolyte decomposition upon cycling. Coupling these two electrodes to make a lithium ion battery is thus highly appealing but also highly difficult because the cell balancing must account not only for the charge reversibly exchanged by each electrode but also for the irreversible charge losses. In this paper a LNMO-nano TiO2 Li-ion cell with liquid electrolyte is presented: two innovative approaches on both the cathode and the anode sides were developed in order to mitigate the electrolyte decomposition upon cycling. In particular the LNMO surface was coated with ZnO in order to minimize the surface reactivity, and the TiO2 nanoparticles where activated by incorporating nano-lithium in the electrode formulation to compensate for the irreversible capacity loss in the first cycle. With these strategies we were able to assemble balanced Li-ion coin cells thus avoiding the use of electrolyte additives and more hazardous and expensive ex-situ SEI preforming chemical or electrochemical procedures. © 2011 Elsevier B.V. |
Notes | cited By 37 |
URL | https://www.scopus.com/inward/record.uri?eid=2-s2.0-80052488913&doi=10.1016%2fj.jpowsour.2011.08.022&partnerID=40&md5=23828504050fdf88acd46b737e8bd4a5 |
DOI | 10.1016/j.jpowsour.2011.08.022 |
Citation Key | Brutti20119792 |